表3 工况划分
Table 3 Grouping of working conditions
分组冻融次数N法向应力/kPa含水率/%含石率/%
0100,200,3002415,25,35,45,55,65
1100,200,3002415,25,35,45,55,65
3100,200,3002415,25,35,45,55,65
5100,200,3002415,25,35,45,55,65
10100,200,3002415,25,35,45,55,65
15100,200,3002415,25,35,45,55,65
20100,200,3002415,25,35,45,55,65